Dissolving Method
Cold Water
Add the flakes in water(30℃)gradually in the proportion of 5%-10%, stir for 2-5mins,leave aside for 1-3 hours, stir again to get even paste, filter it.
Hot Water
Add the flakes in water(25℃-35℃)gradually in the proportion of 5%-10%,heat gradually to the recommended temperature, continue stirring to get even paste, then filter it after cooling down.
Application (10% solution)
Padding:30-80g/L,temperature 30-40℃,one dip & one pad or two dips & two pads, drying and setting.
Dipping:3-8%(o.w.f),temperature 40-60℃,bath ratio 1:10-15,duration in 20-30 mins,hydro-extracted and drying.
Product detail pictures:

Related Product Guide:
Zortrax Apoller Smart Vapor Smoothing Device | Solvent Black 34
West Jefferson names Bryan Crayton next head football coach of the Buccaneers | High Schools | Sulphur Brown 4
We have been convinced that with joint attempts, the business enterprise between us will bring us mutual benefits. We could guarantee you product or service good quality and aggressive value for Popular Design for Active Alumina Zeolite Adsorbent - Softener Flakes – LEADING , The product will supply to all over the world, such as: Latvia, Austria, Argentina, We've been consistently broadening the market within Romania in addition to preparation punching in extra premium quality merchandise connected with printer on t shirt so that you can Romania. Most people firmly believe we've the whole capacity to provide you happy solutions.

It's really lucky to find such a professional and responsible manufacturer, the product quality is good and delivery is timely, very nice.